Metal‑ceramic composite rods are an innovative industrial material that combines the strength of metal with the wear and corrosion resistance of ceramics. With increasing demand for high‑performance materials in manufacturing, metal‑ceramic composites have become critical components for machinery, электроника, и химическая обработка. Chongqing Jifeng Technology specializes in advanced materials and provides high‑performance metal‑ceramic composite rods for industrial upgrading.

  • Подробная информация о продукте
  • Технические характеристики

Advantages of Metal-Ceramic Composites Rod

Ultra-High Wear Resistance

  • Surface hardness HRA 90–95; wear resistance 3–5 times higher than conventional steel, greatly extending service life.

High Temperature & Коррозионная стойкость

  • Withstands temperatures up to 1200°C (in inert atmosphere) and resists strong acids, щелочи, and salt spray.

Легкий & High Stiffness

  • Плотность: 60%–70% of traditional alloys; прочность на сжатие >1500 МПа, ideal for precision instruments.

Wide Application Coverage

  • Suitable for machinery, электроника, энергия, химический, and aerospace fields.

Applications of Metal-Ceramic Composites Rod

Machinery: bearings, guide rails, cutting tools, wear parts

Электроника: semiconductor packaging supports, high-frequency circuit substrates

Энергия & Химическая: pump/seal parts, reactor liners

Аэрокосмическая промышленность: high-temp engine components, легкие конструкции

Why Choose JiFeng Ceramics?

Advanced processes

vacuum hot‑press sintering, plasma spraying

Custom Service

Customizable size, material ratio and surface finishing

Fast delivery

Стандартный 2 weeks; military custom 4–8 weeks.

Full Technical Support

One-stop guidance from selection to installation

ПараметрSpecification
Состав материалаMetal matrix (titanium alloy / stainless steel) + Al₂O₃/ZrO₂ ceramic particles
Плотность4.5–6.2 g/cm³
ТвердостьHRA 90–95
Прочность на сжатие≥1500 MPa
Максимальная рабочая температура≤1200°C (inert atmosphere)
КТР (20–800°C)8.5–11.5×10⁻⁶/°C
Коррозионная стойкостьИСО 9227 salt spray test ≥500 hours